After the blisters have been opened up, we allow them to dry until our moisture meter gives a dry reading.
After the hull is dry, any blister over 1 mat deep will be glassed back up.
Then a 2 part epoxy fairing compound is mixed and faired over the blistered
areas, this is done multiple times until the hull it true and smooth again.
After the filling process comes the barrier coat which is achieve by 5 to 7 coats (depending on the applicator)
of Interlux 2000E Epoxy Primer.
Then the anti-fouling of your choice is top-coated over barrier coat. (3 coats)